PA66 CM3006 日本东丽工业株式会社 物性数据 |
规格级别: | --- | 外观颜色: | --- |
用途概述: | --- | ||
备注说明: | 类型:尼龙-66未强化 |
性能项目 | 试验条件[状态] | 测试方法 |
|
数据单位 | |||||
基本性能 | 吸水率 | 23℃ | ASTM D-570 |
|
% | ||||
物理性能 | 比重 | --- | ASTM D-792 |
|
--- | ||||
泰伯磨耗量 | 1000g,CS-17 | ASTM D-1044 |
|
mg/1000次 | |||||
机械性能 | IZOD冲击强度 | 23℃,无缺口1/2 | --- |
|
kg.cm/cm | ||||
IZOD冲击强度 | 23℃,无缺口1/8 | --- |
|
kg.cm/cm | |||||
洛氏硬度 | 23℃ | ASTM D-785 |
|
R | |||||
洛氏硬度 | 23℃ | ASTM D-785 |
|
--- | |||||
抗拉屈服强度 | -40℃ | ASTM D-638 |
|
Kg/cm2 | |||||
抗拉屈服强度 | 23℃ | ASTM D-638 |
|
Kg/cm2 | |||||
抗拉屈服强度 | 80℃ | ASTM D-638 |
|
Kg/cm2 | |||||
抗拉断裂强度 | 23℃ | ASTM D-638 |
|
Kg/cm2 | |||||
断裂伸长率 | 23℃ | ASTM D-638 |
|
% | |||||
挠曲强度 | -40℃ | ASTM D-790 |
|
Kg/cm2 | |||||
挠曲强度 | 23℃ | ASTM D-790 |
|
Kg/cm2 | |||||
挠曲强度 | 80℃ | ASTM D-790 |
|
Kg/cm2 | |||||
挠曲��量 | -40℃ | ASTM D-790 |
|
Kg/cm2 | |||||
挠曲模量 | 23℃ | ASTM D-790 |
|
Kg/cm2 | |||||
挠曲模量 | 80℃ | ASTM D-790 |
|
Kg/cm2 | |||||
压缩强度 | 23℃ | ASTM D-695 |
|
Kg/cm2 | |||||
抗剪强度 | 23℃ | ASTM D-732 |
|
Kg/cm2 | |||||
IZOD冲击强度 | -40℃,无缺口1/2 | --- |
|
kg.cm/cm | |||||
电气性能 | 体积电阻率 | --- | ASTM D-257 |
|
Ω.cm | ||||
介电常数 | 50HZ | ASTM D-150 |
|
--- | |||||
损耗因素 | 50Hz | ASTM D-150 |
|
--- | |||||
IEC导电径踪指数 | --- | UL 746 |
|
V | |||||
热 性 能 | UL-94抗燃级 | 1/16" | UL 94 |
|
--- | ||||
线性热膨胀系数 | --- | ASTM D-696 |
|
10-5cm/cm | |||||
热挠曲温度 | 4.6kg/cm2 | ASTM D-648 |
|
℃ | |||||
熔点 | --- | 差示扫描测热计DSC法 |
|
℃ | |||||
比热 | --- | --- |
|
Cal/g.°C | |||||
导热系数 | --- | --- |
|
Kcal/m.hr.°C |