AS S695 宁波乐金(LG)甬兴化工有限公司 物性数据 |
规格级别: | --- | 外观颜色: | --- |
用途概述: | --- | ||
备注说明: | 特性:耐化学性 |
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
物理性能 | 比重 | --- | ASTM D-792 | 1.07 | --- |
变缩性 | --- | ASTM D-955 | 0.2~0.6 | % | |
流动系数 | 220℃/5kg | ASTM D-1238 | 3.0 | g/10min | |
流动系数 | 220℃/10kg | ASTM D-1238 | 32 | g/10min | |
机械性能 | 拉伸强度 | --- | ASTM D-638 | 800 | kg/cm2 |
伸长率 | --- | ASTM D-638 | 7 | % | |
弯曲强度 | --- | ASTM D-790 | 1300 | kg/cm2 | |
弯曲模数 | --- | ASTM D-790 | 36,000 | kg/cm2 | |
IZOD冲击强度 | Notched1/4" | ASTM D-256 | 1.5 | kg・cm/cm | |
IZOD冲击强度 | Notched1/8" | ASTM D-256 | 2.0 | kg・cm/cm | |
洛氏硬度 | R-Scale | ASTM D-785 | 122 | --- | |
热 性 能 | 热变形温度 | Unannealed 18.5kg/cm21/2" | ASTM D-648 | 93 | ℃ |
燃烧性 | 1/8" | IEC707 | FH3-25 | mm/min | |
燃烧性 | 1/16" | IEC707 | - | mm/min | |
维卡软化点 | 1,000g | ASTM D-1525 | 110 | ℃ | |
燃烧性 | 1/8" | UL-94 | HB | --- | |
燃烧性 | 1/12" | UL-94 | - | --- | |
燃烧性 | 1/16" | UL-94 | HB | --- |