性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
基本性能 | 熔体流动速率 | --- | ASTM D-1238 | 0.25 | g/10min |
密度 | --- | ASTM D-1505 | 0.9 | g/cm3 | |
OIT | 200℃ | ASTM D-3895 | >30 | min | |
吸水性 | --- | ASTM D-570 | >0.01 | % | |
机械性能 | 屈服拉伸强度 | --- | ASTM D-638 | 230 | kgf/cm2 |
断裂伸长率 | --- | ASTM D-638 | >600 | % | |
弯曲模量 | --- | ASTM D-790 | 8500 | kgf/cm2 | |
洛氏硬度 | --- | ASTM D-785 | 72 | R Scale | |
艾佐德冲击强度 | Non-Notched | ASTM D-256 | NB | kgfcm/cm | |
艾佐德冲击强度 | Notched,23℃ | ASTM D-256 | 60 | kgfcm/cm | |
电气性能 | 体积电阻率 | --- | ASTM D-257 | 1 | 1017Ω.H |
介电常数 | 1KHz | ASTM D-150 | 2.3 | --- | |
耗散(损耗)因数 | 1KHz | ASTM D-150 | 2 | 10-4/℃|10-4/℃ | |
介电强度(短时间) | --- | ASTM D-149 | 40 | KV/М | |
Arc Resistance | --- | ASTM D-495 | 130 | sec | |
热 性 能 | 热传导性 | --- | KPIC Method | 3 | 10-4calcm/cmsec℃ |
热变形温度 | --- | ASTM D-648 | 85 | ℃ | |
比热性 | --- | ASTM D-648 | 0.46 | Ш/g℃ | |
熔点 | --- | ASTM D-3418 | 139 | ℃ | |
维卡软化点 | --- | ASTM D-1525 | 133 | ℃ |