牌号 | N145-LD |
厂家(产地) | 化学 |
POMPOM/N145-LD/LG化学技术数据
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 |
---|---|---|---|---|
吸水率 | ASTM D-570 | 0.22 | 吸水 | |
比重 | ASTM D-792 | 1.41 | ||
磨耗量 | ASTM D-1044 | 14 | mg/1000 cycles | |
模缩系数 | 18~21 | cm/cm×103 | ||
弯曲强度 | ASTM D-790 | 950 | kg/cm2 | |
弯曲模量 | ASTM D-790 | 26000 | kg/cm2 | |
伸长率 | TM D-638 | 45 | % | |
张力 | ASTM D-638 | 610 | kg/cm2 | |
洛氏硬度 | ASTM D-785 | 82 | M(R) | |
岩挤体数(动) | ASTM D-1894 | 0.16 | ||
岩挤体数(静) | ASTM D-1894 | 0.12 | ||
冲击强度(无缺口) | ASTM D-256 | 65 | kg?cm/cm | |
冲击强度(缺口) | ASTM D-256 | 5.5 | kg?cm/cm | |
诱电正接 | ASTM D-150 | 0.007 | ||
介电强度 | ASTM D-149 | 24 | KV/mm | |
介电定数 | ASTM D-150 | 3.8 | ||
抗体积性 | ASTM D-257 | 1×1014 | Ω.cm | |
抗表面性 | ASTM D-257 | 1×1016 | Ω | |
热变形温度 | 4.6kg/cm2 | ASTM D-648 | 160 | ℃ |
缩性热伸张系数 | ASTM D-696 | 10×10-5 | cm/cm/℃ | |
热变形温度 | 18.6kg/cm2 | ASTM D-648 | 110 | ℃ |
燃烧性 | HB(1/32〃) |