TPE 4056 美国杜邦公司 物性数据 |
规格级别: | 高性能级 | 外观颜色: | --- |
用途概述: | 软管护套、电线、电缆护套、薄膜出片、胶带封口。 | ||
备注说明: | 卓越的低温特点,卓越的抗挠曲疲性,卓越的抗蠕变性。 |
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |||||||||
基本性能 | 24小时吸水率 | --- | ASTM D-570 | 0.6 | % | ||||||||
物理性能 | 泰伯磨耗量 | CS-17轮 | ASTM D-1044 | 3 | mg/1000rev | ||||||||
比重 | --- | ASTM D-792 | 1.17 | --- | |||||||||
熔体流动速率 | --- | ASTM D-1238 | 5.3 | g/10min | |||||||||
泰伯磨耗量 | H 18轮 | ASTM D-1044 | 100 | mg/1000rev | |||||||||
机械性能 | 硬度计硬度 | --- | ASTM D-2240 | 40 | --- | ||||||||
揉曲模量 | 23℃ | ASTM D-790 | 62 | MPa | |||||||||
断裂拉伸力 | --- | ASTM D-638 | 28 | MPa | |||||||||
断裂伸长 | --- | ASTM D-638 | 550 | % | |||||||||
|
--- |
|
|
|
|||||||||
埃佐冲击强度 | 23℃ | ASTM D-256 | 不破裂 | J/m | |||||||||
初耐撕裂性能 | --- | ASTM D-1004 | 101 | kn/m | |||||||||
热 性 能 | 熔点 | --- | ASTM D-3418 | 150 | ℃ | ||||||||
维卡软化点 | --- | ASTM D-1525 | 108 | ℃ | |||||||||
热畸变温度 | @0.5MPa | ASTM D-648 | 54 | ℃ | |||||||||
热畸变温度 | @0.18MPa | ASTM D-648 | N/A | ℃ | |||||||||
其它性能 | 耐揉曲切口增长性能 | --- | ASTM D-1052 | >1×106 | --- |